Gentlemen and Ladies,
I am working with a Ductile Iron material (65-45-12): uts-65000 psi, yield pt-45000 psi, elongation-12%. I have a part made from this material, which has a bore and a hole prependicular to the bore. Hole dia is about 1/4 inch and bore diamter is 5 inch. I have carried out a finite element analysis of the part and the maximum stresses occur inside the hole and not at the edge which breaks out in to the bore. This is in line with Peterson's handbook.
Based on the FEA stress concentration inside the hole is 3. I am trying to use Neuber's method for analysis of notches. But I do not have the material constant A required for Nueber's formula. However I found a graph in Ductile Iron Handbook, which plots the S-N curves for a notched and un-notched sample (bar with a v-groove notch). Based on this Kf value is 1.67. The root radius is 0.01 inch. I ran an axi-symmetrical analysis to find out the Kt value for the notch. Using a very fine mesh and ensuring convergence I found Kt = 11.
I calculated the sqrt(A) for Neuber's method and come up with a value of 1.4 inch for the material. The value does not seem to be reasonable. Please give me your comments on above.
Gurmeet
I am working with a Ductile Iron material (65-45-12): uts-65000 psi, yield pt-45000 psi, elongation-12%. I have a part made from this material, which has a bore and a hole prependicular to the bore. Hole dia is about 1/4 inch and bore diamter is 5 inch. I have carried out a finite element analysis of the part and the maximum stresses occur inside the hole and not at the edge which breaks out in to the bore. This is in line with Peterson's handbook.
Based on the FEA stress concentration inside the hole is 3. I am trying to use Neuber's method for analysis of notches. But I do not have the material constant A required for Nueber's formula. However I found a graph in Ductile Iron Handbook, which plots the S-N curves for a notched and un-notched sample (bar with a v-groove notch). Based on this Kf value is 1.67. The root radius is 0.01 inch. I ran an axi-symmetrical analysis to find out the Kt value for the notch. Using a very fine mesh and ensuring convergence I found Kt = 11.
I calculated the sqrt(A) for Neuber's method and come up with a value of 1.4 inch for the material. The value does not seem to be reasonable. Please give me your comments on above.
Gurmeet