We currently use 1026 ASTM A513-00 Type 5, 6.25" OD x 3/8" wall DOM Round Tube, Normalized with following specs.
Yield = 48,330 ksi
Ultimate = 71,070 ksi
% Elong in 2" = 33.9
HRB = 75-76
Our supplier is out of stock on this material & wants to substitute material with the following specs.
Material was normalized, but then was heat treated again (unkown process)
Yield = 78,000 ksi
Ultimate = 92,000 ksi
% Elong in 2" = 25
HRB = 92
For our process I'm concerned about the impact of the elevated hardness.
Any Thoughts! Thanks
Neil
We currently use 1026 ASTM A513-00 Type 5, 6.25" OD x 3/8" wall DOM Round Tube, Normalized with following specs.
Yield = 48,330 ksi
Ultimate = 71,070 ksi
% Elong in 2" = 33.9
HRB = 75-76
Our supplier is out of stock on this material & wants to substitute material with the following specs.
Material was normalized, but then was heat treated again (unkown process)
Yield = 78,000 ksi
Ultimate = 92,000 ksi
% Elong in 2" = 25
HRB = 92
For our process I'm concerned about the impact of the elevated hardness.
Any Thoughts! Thanks
Neil