I am working on the design of a clip that will be used in our manufacturing process to help stabilize the corners of some flimsy frames.

It is basically a corner clip that will snap into the frame to help hold the corner square. It will be used a couple of times and then thrown away. It will be on the frame for about an hour at the most and then removed during assembly.

The clip is about 1.5" square and about .100" thick (through the support). It needs to be somewhat flexible in order to snap in, but ridgid enough to support the frame.

Thanks!
Joe
 
Joe

You do not give anywhere near enough information for me to hazard a guess.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Joe,
We make a similar clip out of POLYPRO in house. we use some simple tooling for small runs. Our website is Drop me an email if you would like to talk/share design/production tips @ mharp@chemcut.net
 
Joe,
What exactly is your question? Material selectio? Snap design?....
 
Sorry, the title was supposed to be "Material for disposable clip".

I am meeting with a plastic manufacturer this morning to move the project forward. I will keep you guys posted on what I end up with.