okay here sia method we used, for castings, as well as coatings. On a refular basis, we blasted the dies with not sand or abrasive material but dry ice, this removed all crud and left die clean. it also reduced die temps.
its quite expensive, but compared to time lost lifitng out dies to clean them its a good cost saving.