In my understanding, the markings on each length of pipe shall
include the plate material designations. This is a requirement of ASTM A 358.
If the actual marking shows only heat number without plate material designation , can we accept this pipe material?
Is this the normal practice in steel manufacturing industry?
Please comment.
include the plate material designations. This is a requirement of ASTM A 358.
If the actual marking shows only heat number without plate material designation , can we accept this pipe material?
Is this the normal practice in steel manufacturing industry?
Please comment.