We have ordered boltings in L7 ASTM A320 but with an impact test at minus 20°C instead of standard minus 101°C because minus 20°C is our intended service temperature.
We do not know:
1. what would be the stamping of the pieces?
2. what must be written on the materail certificate as to distinguish fro the standar L7 impact test at minus 101°C?
3. Where is clearly indicated on the ASTM standards how mast be marke and certified?
I read ASTM A320, A370 and A962 without find clearly indications.
On ASTM A320 para. 6.2.1.1 is generically indicated " ..... and the bolting is suitably marked to identify the reported test temperature""
Thanks for you help
V.Federella
We do not know:
1. what would be the stamping of the pieces?
2. what must be written on the materail certificate as to distinguish fro the standar L7 impact test at minus 101°C?
3. Where is clearly indicated on the ASTM standards how mast be marke and certified?
I read ASTM A320, A370 and A962 without find clearly indications.
On ASTM A320 para. 6.2.1.1 is generically indicated " ..... and the bolting is suitably marked to identify the reported test temperature""
Thanks for you help
V.Federella