Hello,

i were badly looking for Maraging steel for one of my
aeropsace product.Can any one suggest me
maraging steel manufacturing or distrubuting
companies list around the world.

Thanx in before

John
 
Matweb has 71 listings for maraging steels. [click 'Materials Type,' then under "Ferrous Metals,' scroll down to 'Maraging Steels' & click 'Find.']
Most are listed by AISI designation (generics). Those listed by manufacturer are:

Vasco® 9-4-30 Specialty Steel, Heat Treatment: 899°C (1650°F) + Age
VascoMax® C-250 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age
VascoMax® C-300 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age
VascoMax® C-350 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age
VascoMax® T-250 Specialty Steel, Heat Treatment: 816°C (1500°F) + Age

Special Metals UDIMET® Alloy 250 Maraging Steel

Timken Latrobe Marvac® 250 VIM-VAR; 10 in. High Strength Maraging Steel
Timken Latrobe Marvac® 250 VIM-VAR; 5 in. High Strength Maraging Steel
Timken Latrobe Marvac® 300 VIM-VAR; 10 in. High Strength Maraging Steel
Timken Latrobe Marvac® 300 VIM-VAR; 6.25 in. High Strength Maraging Steel
Timken Latrobe Marvac® 300 VIM-VAR; 5 RCS High Strength Maraging Steel
 
To continue with Ken's information,

Vasco & VascoMax are from Allegheny Technologies:


Special Metals' maraging steel is UDIMAR:


And Timken's Marvac is here:


Regards,

Cory