I've seen several good posts on composite bladder molding, but I'm wondering if anyone has some specific recommendations for:
1) Silicone materials, sources, methods to use to make the bladders
2) Wall thickness of the bladder
FYI we can't used a trapped solid rubber mandrel since it would be trapped in the mold due to the bends in the part.
Thanks
1) Silicone materials, sources, methods to use to make the bladders
2) Wall thickness of the bladder
FYI we can't used a trapped solid rubber mandrel since it would be trapped in the mold due to the bends in the part.
Thanks