marceloneavez
Mechanical
I have to fix the seat on a valve that is not produced anymore nor the valve or the spares. This is a three piece trunnion supportes ball valve, this valves have the seat ( Reinforced PTFE) integrated with a seat holder made of A105N/ENP so in order to change the seat i have to be able to found another seat holder with the seat integrated the problem is that they dont produce anymore of them. I found a diferent brand PBV wich have the same design on the valve but im not shure if it will work. Any sugestions on this topic?