Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Magnetic B-H Curves

Status
Not open for further replies.

SnappyP

Materials
Mar 12, 2008
1
I am new to the magnetics world, but working on a solenoid and want to know what type of equipment is used to generate B-H Curves. Also, who would be a leading supplier of that equipment and the estimated cost. The solenoid requires a little more (10%) pull-in force midway through its travel and I am considering a full anneal of the armature and pole piece, but I need a baseline of the existing parts as they are today. The pole is 1018 and the armature is 12L14 Steel.
 
Replies continue below

Recommended for you

Magnetic Instrumentation is another source

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
You do not need much to record an AC hysterisis curve. I have used a low voltage AC source (adjustable transformer) and an oscilloscope with integrating function. The TiePie HS4, for instance, has a very flexible set of "functions" that can be used for almost any measurement.

The attached picture shows measurements on a toroid made from ferrite. The saturation flux can be easily calculated from the results. As can many other properties.