I am trying to verify a customers design of a magazine spring. The spring dimensions are as follows:

Material: Music wire
Wire diameter 0.032"
Width ID .775"
Height ID .157"
Free length 4.85"
Total coils 12

Looking for forces at heights 2.798" & .890". I have attached a drawing for reference