We are machining some bushings made from S355J0, a structural steel, and having some problems. Here's the deal:
Material: 125mm hot-rolled bar stock
Part: 121mm OD, 106mm ID (+.0016) x 35mm long
Prep: Saw-cut with 3/16" stock on length and pre-drilling a 1-5/16 hole.
We machined one part and it went out-of-round over night!
Does this material need to be normalized before machining? Should we rough it out, normalize, and then finish?
Any help would be most appreciated!!
Thanks,
Wganders
Material: 125mm hot-rolled bar stock
Part: 121mm OD, 106mm ID (+.0016) x 35mm long
Prep: Saw-cut with 3/16" stock on length and pre-drilling a 1-5/16 hole.
We machined one part and it went out-of-round over night!
Does this material need to be normalized before machining? Should we rough it out, normalize, and then finish?
Any help would be most appreciated!!
Thanks,
Wganders