Machining polypropylene with 20 - 40% calcium carbonate in it?

I would appreciate any information. Tradenames of material, feeds and speeds, etc.

Thanks,
Tom

Thomas J. Walz
Carbide Processors, Inc.

Good engineering starts with a Grainger Catalog.
 
For neat PP:
HSS may be a better choice than carbide.
Lots of positive rake, lots of clearance, and a polished, razor sharp edge.
Minimum depth of cut ~.005" or a bit more. You can't shave just a little.
Low-ish speeds.
Refrigeration of the workpiece and/or a stream of cold air on the tool may help.

With CaCO3, you might need to sharpen the edge more often.


Mike Halloran
Pembroke Pines, FL, USA
 
Thank you, Sir.

We thought about steel but it for a manufacturing plant and we are afraid steel will wear too fast.

We are going with a sub micron grade which will take a very good edge.

Narrow plate and relatively wide side clearance to suck air through.

Maybe an ATAF (altenate top / alternate face) to minimize contact between tip and material.

Also we need to maintain a sharp edge and the top, decorative layer is fibrous and comes off in strings.