I face a problem right now:to make a 1/4-16 ACME internal thread,material for the part is stainless steel, Minor diameter is only about 0.1875-0.1925, I have tried both drill & tap and cutting method, but can not get good result.
Are there any other method to make it? or maybe there are some tips on tapping or cutting.

Thanks!
 
Replies continue below

Recommended for you

Try a google search for 'micro 100'. They make excellent carbide tools for your purpose.
 
I have got contact with micro 100 and ordered 10 cutter for trial, thanks for your information.
 