Considering surface texture terms (roughness, waviness, lay),
The machining marks resulting from a machining process - not from chatter or workpiece stability issues, but only from factors as the cutting edge nose radius and machining feed - do they get detected as a roughness profile?
Or could they as well be measured as waviness (filtered to exclude a more closely spaced interruptions that are labeled as roughness)?
 
Replies continue below

Recommended for you

There's nothing special about marks from machines operations, they're part of the surface and thus controlled by surface descriptors in GD&T on the part print - roughness, flatness, cylindricality, etc.

On the rare occasion where you legitimately need to specify details of the manufacturing process and are willing to accept the additional costs, then you need a separate manufacturing process print.
 