Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

machining glass

Status
Not open for further replies.

josson

Mechanical
Dec 9, 2004
12
Can glass (specifically borosilicate) be machined using typical processes or are there special consideriations and processes required.

 
Replies continue below

Recommended for you

If the tension -- the sum of the externally applied and of
the innner tension -- exceeds the tensile strength, the glass breaks.

It means the machnining must not create large tension
or else you must remove the inner tension with heat treatment. You can visualize the inner tension with
polarized light.




<nbucska@pcperipherals DOT com> subj: eng-tips
read FAQ240-1032
 