I have a heat sink that i want to insert two cartridge type heaters. Unfortunately the heat sink profiles i have found that fit my assembly do not leave much surrounding material if i drill it out for the cartridge heaters.
I have to drill a 1/8" hole about 1.5" to 2" deep. The surrounding thickness will be about 3/64". My question is, How much should i expect the drill bit to wander?
Is there a rule of thumb that says X diameters deep is the maximum depth with accuracy? My supervisor suggested 3 diameters but that seems very minute.