Hi all!
Fabrication of 36" Pressure Vessel has been completed. This vessel has a support ring that is welded inside the vessel shell. This ring will support the tube plate.
Vessel is about to be hydrotested.
Just now we found out that we have to modify the support ring.
Can we machine support ring after the hydrotest of vessel?
If we postpone the hydrotest, it could lead to delays.
Regards,
PEHasan.