Mar 12, 2002 #1 vivaldi Mechanical Joined Feb 19, 2002 Messages 6 Location SE How can I machine a titanium conical screw which has a taper angle 22 degree and a pitch 0.8mm (Number of revolutions=4)? Regards,
How can I machine a titanium conical screw which has a taper angle 22 degree and a pitch 0.8mm (Number of revolutions=4)? Regards,
Mar 12, 2002 #2 sbc Automotive Joined Dec 7, 2001 Messages 56 Location US A lathe with a taper attatchment should do the trick. Upvote 0 Downvote
Mar 25, 2002 #3 Guest you didn't say if the 22 deg angle was included or single side. if single side, I doubt a taper attachment will accomodate you very well. this is easiest to do on cnc. Upvote 0 Downvote