I have a piece of 0.25" 17-4 plate that forms a Z shape (approx. 7" long and 2" high with web of 3/16" thick). I had the plate treated to approx H900. I waterjet cut the Z shape. I then had to mill 0.06" off most of one side. The part warped 0.05". I had the material (Z-shaped parts) tempered back to the annealed state and milled another piece and it warped about 0.035". Any ideas? I am taking the 0.060" off in one pass. Could I be building up to much heat?