Can any one suggest, or help point me in the direction of, information that will enable me to decide on a Machining surface finish for a selection of small aluminium components that require Anodising.
The anodising I intend to use is Sulphuric - Dyed in various colours, and serves 2 purposes:
1. Eliminate the possibility of electrolytic reaction in a mixed metal water-cooling system.
2. To improve the visual appearance of the components.
The components can't be subjected to extensive etching due to the risk of eroding Small tapped threads. Therefore I am looking to specify a machined finish that will enhance the final anodised finish.
I don't currently have access to gauging or visual references of surface finishes but from what information I have found, I’ve been tempted to use a finish of 64 MicroInch but am hesitant until I can establish this value is ideal, and how it will effect machining.
Thanks in advance
The anodising I intend to use is Sulphuric - Dyed in various colours, and serves 2 purposes:
1. Eliminate the possibility of electrolytic reaction in a mixed metal water-cooling system.
2. To improve the visual appearance of the components.
The components can't be subjected to extensive etching due to the risk of eroding Small tapped threads. Therefore I am looking to specify a machined finish that will enhance the final anodised finish.
I don't currently have access to gauging or visual references of surface finishes but from what information I have found, I’ve been tempted to use a finish of 64 MicroInch but am hesitant until I can establish this value is ideal, and how it will effect machining.
Thanks in advance