Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Machine Screw Pull-Out Capacity 1

Gerrha

Chemical
Joined
Dec 3, 2006
Messages
8
Location
USA
I am a retired scientist and off/on for many years I planned to build a small liquid fuel rocket engine. My son recently got me interested again so I am back working on the project. This engine will never leave the ground. It is for fun and also for my son and I to learn many new things along the way. As a starting point, the design will have a combustion chamber with a round injector plate on the top. They will be bolted together. These parts are fairly small, less than 3" in diameter, so the screws also need to be small as in #4 through maybe #8. Our current design would use 8, 6-32 socket-head cap screws with a thread engagement of 1/2". The material is copper, and the chamber pressure is 500-psig. The thing will be operated remotely, so if it blows up no harm will be done, but the point of the project is to learn what is required for a proper design. This bolt arrangement has become a question for me. It looks good on paper, but from an engineering consideration, is our bolt arrangement adequate or not?

I have searched many sources and cannot find this type of information. However, it must be out there somewhere. Could someone please help us with this?
 
It's hard to give crisp answers because I can't visualize what you're showing.

The primary questions are:
1) will the applied load put the screws be in shear or pure tensile/tear-out?
2) how flat and consistent will the mating surfaces be under the screws?
3) what strength is expected for the screw material and for the copper?
4) when you say 1/2" thread engagement and screws, those keywords have me visualizing a tapped hole in solid copper that is deeper than 1/2" and has the screw engaging 1/2". Please confirm this is correct as opposed to a screw/nut setup.

I can offer that for standard steel bolts screwed directly into tapped holes in soft materials like copper, I would aim to have (1.5x to 2.0x screw diameters) of thread engagement. This follows rules of thumb that say the full tearout strength is reached in 1.0-1.25x for high strength materials and more engagement is required for lower strength materials. 1/2" seems like more than enough there.
 
Thanks for your reply. Your questions are all things I have thought about as well and this is what I can answer.

1. Pure tear-out tensile. There should not be any shear.
2. The surfaces will be flat and very smooth because there will be o-rings involved to keep the combustion gases where they are supposed to be. The surface finish will be specified at Ra 16.
3. The screws planned as of now, will be stainless steel A286 with 160K psi tensile strength and 120K psi yield strength. I have assumed 10K PSI yield strength for the copper.
4. You are correct in that the plan is for blind tapped holes in the solid copper injector plate that are deep enough to provide 1/2" thread engagement. This depth can be adjusted if needed. Also, the tap used will be selected to provide 75% thread. For the planned 6-32 screw, this is a tap drill of 0.1065" diameter.

Thanks!
 
I had a similar conundrum a few years back on a project, couldn't find any data so just ended up having to do my own tests.

Agreed with dgeesaman, if you have 1/2" engagement I would suspect that would be plenty. Wouldn't surprise me if you broke the bolt before getting it to pull out. Assuming pure tension loads of course.
 
There must be some sort of guidance out there.

There is an o-ring seal between the combustion chamber and injector plate. The OD of that o-ring is 2.637" and the chamber pressure at maximum engine capacity is 500-psig. That will equate to about 2750-lbs of force pushing those two plates apart. There must be some way to determine the number of 6-32 screws (4, 6, 8, 12?) that will be safe under those conditions or maybe not safe at all and a larger screw is needed.
 
Thanks for that link and information. It took me a while to go through it.

Here is what I calculated for a 6-32 screw used in a situation like this. I hope it is correct. I feel I am on very thin ice with the final three calculations (highlighted below), which were not in the link. I sort of made the final three calculations based on what seemed logical to me, but I am not sure. If what I have is correct, then in theory, two 6-32 screws would be sufficient for my expected 2750 pounds. I plan to use 8. Does that make sense? Also, the calculations show that a thread engagement length of 0.36" should be adequate and I plan for 0.5".

Thanks for the help!



Parameter6-32 screwCalculation
D, basic screw diameter, inch0.138Given
TPI, threads/inch, inch-132Given
Ts, screw material tensile strength, psi160000Given
Cs, copper tensile strength, psi45000Given
P, thread pitch, inch0.03125P = 1/TPI
At, tensile stress area, inch2 0.00927685At = p * (D - 0.938194 * P)2/4
Ds, tensile stress diameter, inch0.10868144Ds = 2 * (At/p)1/2
Dp, pitch circle diameter, inch0.1177025Dp = D - 0.64952 * P
Le, length of thread, screw, inch0.10Le = 2 * At/(0.5 * p * Dp)
Asss, thread shear area, screw, inch20.0185537Asss = Le * 0.5 * p * Dp
J, material strength factor, unitless3.56J = Ts/Cs
Le2, length of thread, copper, inch0.36Le2 = J * Le
Assc, thread shear area, copper, inch20.06596873Assc = Le2 * 0.5 * p * Dp
Ss, strength, screw, lbs1484Ss = Ts * At
Sst, strength, screw threads, lbs2969Sst = Ts * Asss
Sct, strength, copper threads, lbs2969Sct = Cs * Assc
 
I think that 45ski for Cu is being optimistic, 32ksi is more appropriate unless you have a specific alloy in mind.
And the yield will only be 10-15ksi
 
Thanks, that is good information. If I use 32 ksi for the copper, the updated table is shown below. This ups the required thread engagement length to 0.5" which is what I was planning all along. That is good news - assuming my calcs above are correct.

Are the final three calculations correct? What they tell me is that the screw will break before the threads will pullout and that a single screw can take approximately 1450 pounds of tension before breaking. That seems to me a lot of force for a small 6-32 screw.



Parameter6-32 screwCalculation
D, basic screw diameter, inch0.138Given
TPI, threads/inch, inch-132Given
Ts, screw material tensile strength, psi160000Given
Cs, copper tensile strength, psi32000Given
P, thread pitch, inch0.03125P = 1/TPI
At, tensile stress area, inch2 0.00927685At = p * (D - 0.938194 * P)2/4
Ds, tensile stress diameter, inch0.10868144Ds = 2 * (At/p)1/2
Dp, pitch circle diameter, inch0.1177025Dp = D - 0.64952 * P
Le, length of thread, screw, inch0.10Le = 2 * At/(0.5 * p * Dp)
Asss, thread shear area, screw, inch20.0185537Asss = Le * 0.5 * p * Dp
J, material strength factor, unitless5.00J = Ts/Cs
Le2, length of thread, copper, inch0.50Le2 = J * Le
Assc, thread shear area, copper, inch20.09276852Assc = Le2 * 0.5 * p * Dp
Ss, strength, screw, lbs1484Ss = Ts * At
Sst, strength, screw threads, lbs2969Sst = Ts * Asss
Sct, strength, copper threads, lbs2969Sct = Cs * Assc
 
I slammed #6-32 / A286 data into my bolt calculator and got 1300# of preload so that seems about right. Screws (esp. high strength screws in high strength materials) can generate very high tensile loads.

Personally I'd prefer to assume lower utilization than that and have a factor of safety of 1.5.

Are either of the faces being bolted together somewhat thin? In other words, the compression of the screw is highest directly under the screw head and if you're bolting down a thin plate/flange there may be very little compression in between the bolts. The copper side with tapped holes seems pretty thick so I'm asking about the other side. O-rings have compression even if the metal parts surrounding them aren't pressed tightly together, but if one side is thin enough the screw torque can distort the thin side and reduce sealing capacity.
 
The o-ring is a size 229 with OD at 2.637". The plan has 8, 6-32 screws arranged in a circle pattern 45-degrees apart around the outside of the o-ring. The screw circle is 3.098" diameter. Both parts are copper with the upper injector plate 0.75" thick. This has the tapped holes with 0.5" thread engagement.

The lower, combustion chamber, has the through holes that are 0.144" in diameter. The thickness of that area is 0.3" but could be thicker if needed. I was also planning to use a washer for each screw that is made of 17-4 PH stainless. They are 0.312" diameter with a 0.156" through hole and 0.038" thick. My idea here was to spread out the area of contact and prevent damage to the soft copper.
 
Thread pull out is a shear failure. For copper, more in the neighborhood of 25,000 psi, depending on type and hardness.

You'll not get equal load distribution over 0.5 inch of thread engagement. At least not initially. After the first load cycle as things yield the distribution will improve, but using the full 0.5 length in a calculation is optimistic. Maybe 5 threads, or 0.15 inch engagement.

So, you're maybe in the ballpark of 1,400 pounds pull out strength for a tapped hole in "copper".

You can't assume that the screws will share the load evenly.

Probably ok, at normal temperatures.

But, it's a rocket, so heat cycles. Thermal expansion of copper and the SS screws is very different.

Lots of assumptions in the above. Test it if you really want to know.
 
Just out of interest, I find myself trying to think of possible loading cases. I've never done anything like this, so my brain-storming could be completely wrong! I start to think, is there any possibility of conditions like 'irregular fuel burn' within the exhaust chamber. I'm wondering if some form of pressure differential could occur (time related), causing side (shear) loads? Sometimes my thoughts do start to wonder!
 
Thread pull out is a shear failure. For copper, more in the neighborhood of 25,000 psi, depending on type and hardness.

You'll not get equal load distribution over 0.5 inch of thread engagement. At least not initially. After the first load cycle as things yield the distribution will improve, but using the full 0.5 length in a calculation is optimistic. Maybe 5 threads, or 0.15 inch engagement.

So, you're maybe in the ballpark of 1,400 pounds pull out strength for a tapped hole in "copper".

You can't assume that the screws will share the load evenly.

Probably ok, at normal temperatures.

But, it's a rocket, so heat cycles. Thermal expansion of copper and the SS screws is very different.

Lots of assumptions in the above. Test it if you really want to know.
I agree - lots of assumptions here and actual testing is the only way to find out. But I am very happy to have received this feedback because it gives me a basis for our starting point and for what we hope to do and achieve. I had not thought about thermal expansion differences between the copper and screws. I will check that out. The good news is that the engine run times are very short, 30-seconds would be very long. In addition, the entire thing is enclosed in a brass jacket with water flowing around it for cooling.
 
With our sim
Just out of interest, I find myself trying to think of possible loading cases. I've never done anything like this, so my brain-storming could be completely wrong! I start to think, is there any possibility of conditions like 'irregular fuel burn' within the exhaust chamber. I'm wondering if some form of pressure differential could occur (time related), causing side (shear) loads? Sometimes my thoughts do start to wonder!
Our design is pretty simple and based on a design that was tested many times back in the 1960s and probably many times since then. However, being relatively simple, the probability of irregular propellant mixing and combustion is likely quite high. Atomization of the propellants is very important for good stable combustion. We already know this will be an issue with this design because the fuel is a liquid and the oxidizer is a gas. Under this situation, there is no feasible way to fabricate an impingement strategy that would provide highly efficient atomization. There will likely be pressure surges and other unpredictable combustion-related things going on, meaning - the entire thing might just blow up in the first seconds. Hopefully, we will get to find out.
 