I am designing a heat staking fixture (inserts brass inserts into thermoplastic parts with the aid of heat) for the injection molding industry. The staking procedure requires temperatures of around 300 degrees F and the machine can handle a max of around 1000 degrees F as long as insulation is present between the heated probe tips and upper carriage. This insulation is generally 1" thick, but the identity of the material is kept proprietary by many manufacturers. The insulation must be MACHINABLE and able to withstand approx. 100psi. Does Macor sound like a probable alternative? Does anyone know of a cheap material that should be able to perform well in these conditions. I've attached a photo of a similar fixture for reference. The insulation is the layer sandwiched between the two aluminum plates.