I AM TRYING TO CUT BACK THE THREADED LENGTH ON A 8.8 BOLT WITH A M6X1.0 THREAD FROM 35MM TO 32MM.AM DOING THIS ON A AUTOMATIC SCREW MACINE,LIKE A LATHE.I AM HAVING PROBLEMS RELEADING THE THREAD DUE TO FLAG LIKE BURRS.ANY SUGGESTION ON CUTTING SFM OR ANY SUGGESTION WOULD BE HELPFUL
 