Hi,
I am looking for a material in solid sheet (or solid board) form:
- Thickness: Between 1/4 and 1/2 inches,
- Continious working temperature: 180F, no outgassing at this temperature
- Water proof, no or very low absorbance of water,
- Machineable with std tools,
- Accepts/adheres with silicone based adhesives, (after primer application),
- Very low Linear thermal expansion, close to glass, which is around 9 (10-6 m/(m K)
- Thermal insulation is a plus,
- Electrically insulative, and no metals or carbon in material,
- Commercial availability and acceptable cost,
Questions welcomed,
Thanks in advance, I appreciate all thoughts, suggestions and questions,
Jakelian
I am looking for a material in solid sheet (or solid board) form:
- Thickness: Between 1/4 and 1/2 inches,
- Continious working temperature: 180F, no outgassing at this temperature
- Water proof, no or very low absorbance of water,
- Machineable with std tools,
- Accepts/adheres with silicone based adhesives, (after primer application),
- Very low Linear thermal expansion, close to glass, which is around 9 (10-6 m/(m K)
- Thermal insulation is a plus,
- Electrically insulative, and no metals or carbon in material,
- Commercial availability and acceptable cost,
Questions welcomed,
Thanks in advance, I appreciate all thoughts, suggestions and questions,
Jakelian