Hi,

I would appreciate your help on ASME VIII Div 1:

The scenario is: Carbon steel vessel with thickness of 60 mm and a minimum T of - 70°C during depressurization. Based on ASME VIII Div 1 UCS-66 is possible an exemption of impact test because the stress ratio is lower than 0.35.
Is the exemption applicable also to the weld metal?

Thanks in advance
Regards
V.
 
Replies continue below

Recommended for you

Is this stress ratio based on vessel at MAWP ( without taking credit for corrosion allowance) or depressurisation final pressure?
 