In the UK we have Ultra Low Sulphur Fuel
The feature of the invention is that the use of a low sulphur fuel enables the amount of anti-wear agents containing phosphorus such as eg ZDDP to be halved without any adverse effect on the antiwear performance of the lubricating oil.
Is the fuel quality a major player in the general ZDDP reduction for anti wear?
The feature of the invention is that the use of a low sulphur fuel enables the amount of anti-wear agents containing phosphorus such as eg ZDDP to be halved without any adverse effect on the antiwear performance of the lubricating oil.
Is the fuel quality a major player in the general ZDDP reduction for anti wear?