we receive P91 elbows Brinnel Hardness 134-137. Straight pipe has HB 184-232.
Is this HB acceptable for 24" sch 40 elbow designed to 20 years , temperature 532 oC and pressure 36 bar ?
On what others parameters this impact?
What to do to correct this?