Hello everyone, I would like to request support from the experts on this matter. We are switching from certain phenolic prepreg to a different one available from same manufacturer which mentions both are the same. We perform Hardness test per our own specification which request an average of 68-75 we are testing this new material, and we are getting Hardness results as low as 50 and maximum of 70. We changed the recipe and increase the soak time up the maximum requested by the manufacturer, also performed different bagging methods in order to attempt to increase Barcol Hardness results without much good results. We also are checking ASTM D2583, which it calls for a Polyester Laminate and its average request is 55. Is there any other way to attempt to increase Barcol Hardness results on them or should we attempt to perform testings to come up with a base line and modify our own specification to reduce it to whatever the results we get?
Please advice ! Thanks a lot !