aladdin76,
Is the PT to the beams, UNbonded or bonded (grouted)?
What other characteristics are evident to the beams that necessitate "...beams to be checked for tension loss"?
I agree with rowingengineer, horizontal cracking to beam webs are not usually associated with loss of prestress, HOWEVER, if the tendons were incorrectly draped (sharp curvature over short lengths, for example) it is possible that horizontal cracking can occur during/shortly after stressing.