knowlittle
Materials
- Jul 26, 2007
- 192
I need to place a metal cylinder (1" dia x 10" long) insider another metal cylinder. I am looking for a rigid, thermally conductive material to fill the gap. I found boron nitride filled epoxy is the best among epoxies. Can I buy this epoxy and add additional metal particles for even better heat conduction?