Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Looking for teflon paste

Status
Not open for further replies.

MechEngr07

Mechanical
Joined
Feb 15, 2010
Messages
9
Location
US
Many years ago (40, I hate to say), a fellow I knew had a can of teflon paste (for lack of a better word). It came in a quart paint type can. The paste was a light green in color. The paste itself was very granular. He told me it would quiet any mating gears, but could only be used in a 'splash' type oiling system. It was applies with a paint brush on the mating surfaces of the gears.

I have searched many places and ask several people, but I have had no luck finding it. Any help would be appreciated.
 
my neighbor is a plumber and uses a product like that
didn't look like this, but same description would apply:

or this
High pressure PTFE lubrication paste
Lubrication of plastic gears at low and high temperatures as well as low to medium speeds. Long-term lubrication of heavily loaded small gears. Good corrosion protection. Good compatibility to plastics. Plastic gears in roller-shutter and awning drives.

 
I sold the raw materials to the likes of Nulon and Slick 50 back in the day. We advised them that the use of PTFE in such circumstances was of very doubtful value as it does not stick to the surface and may block or restrict oil flow to some areas. Oil flow is often necessary for cooling as well as lubrication.

In my opinion a paste product merely takes up clearance much like banana skins.