floattuber
Mechanical
We need to build an impromptu temperature chamber for our shake table which goes up to approximately 350F. The size will only be about 30"x19"x17". Ideally, we'd like to use a rigid foam insulation like the type used for houses, but they only go up to about 250F.
Mcmaster has rigid fiberglass insulation (page 3418)in which the insulation itself is rated up to 450F, but the facing can only go up to 150F, so that is out.
We were going to go with Marinite, but I've now been told it could be hard to get.
Anybody have any suggestions?
Mcmaster has rigid fiberglass insulation (page 3418)in which the insulation itself is rated up to 450F, but the facing can only go up to 150F, so that is out.
We were going to go with Marinite, but I've now been told it could be hard to get.
Anybody have any suggestions?