If this is only a "form Deck", it is typically designed only to take the dead load of the wet concrete plus a nominal construction load. The slab would then be designed and reinforced to take all the dead and live loads. Typically,fprmdeck is only 3/4" to 1" in depth.
If this is what you are looking for, I found design tables in my Vulcraft catqalogues for this material. Perhaps you need to contact Vulcraft to update your manuals or pbtain additional catalogues.
There are other decks designed to be composite, but they are much deeper at 1.5" to 6".
Mike McCann
MMC Engineering