Apr 18, 2006 #1 redhand Civil/Environmental Joined Jan 5, 2004 Messages 12 Location CA Hello, Does anyone know where one could purchase flat sheet membrane that has NOT been configured into anything like a spiral or put in a system yet? Thanks for any advice
Hello, Does anyone know where one could purchase flat sheet membrane that has NOT been configured into anything like a spiral or put in a system yet? Thanks for any advice
Apr 20, 2006 #2 scholles Chemical Joined Apr 20, 2006 Messages 1 Location DE Hello redhand, try to ask GKSS Reserch center in Geesthacht Germany. They develop new materials for all membrane application. http://www.gkss.deInstitut for polymer research Upvote 0 Downvote
Hello redhand, try to ask GKSS Reserch center in Geesthacht Germany. They develop new materials for all membrane application. http://www.gkss.deInstitut for polymer research
Jul 4, 2006 #3 hprorelis Materials Joined Oct 3, 2005 Messages 14 Location FR Hello redhand ORELIS (France) from Novasep group produce flat sheet membrane since many years Check Novasep web site Best regards Upvote 0 Downvote
Hello redhand ORELIS (France) from Novasep group produce flat sheet membrane since many years Check Novasep web site Best regards
Aug 30, 2006 #4 hprorelis Materials Joined Oct 3, 2005 Messages 14 Location FR ORELIS (Novasep Group) in France produce flat sheet membrane - this membrane can be used for plate and frame module and/or spiral module. Upvote 0 Downvote
ORELIS (Novasep Group) in France produce flat sheet membrane - this membrane can be used for plate and frame module and/or spiral module.