Aug 30, 2017 #1 SNORGY Mechanical Joined Sep 14, 2005 Messages 2,510 Location CA I am just checking a Code calculation for tubes in a Section I boiler. The S values from 500 F to 800 F would be useful; I do have the 2010 Code values. Many thanks in advance... Who is right doesn't matter. What is right is all that matters.
I am just checking a Code calculation for tubes in a Section I boiler. The S values from 500 F to 800 F would be useful; I do have the 2010 Code values. Many thanks in advance... Who is right doesn't matter. What is right is all that matters.
Aug 31, 2017 1 #2 pdiculous963 Mechanical Joined May 7, 2012 Messages 122 Location US Here you go: [ul] [li]Ambient to 650F: 15 ksi [/li] [li]700: 14.4 ksi [/li] [li]750: 13 ksi [/li] [li]800F: 10.8 ksi [/li] [/ul] Upvote 0 Downvote
Here you go: [ul] [li]Ambient to 650F: 15 ksi [/li] [li]700: 14.4 ksi [/li] [li]750: 13 ksi [/li] [li]800F: 10.8 ksi [/li] [/ul]
Aug 31, 2017 Thread starter #3 SNORGY Mechanical Joined Sep 14, 2005 Messages 2,510 Location CA pdiculous963, Thank you! Exactly what I needed. Who is right doesn't matter. What is right is all that matters. Upvote 0 Downvote
pdiculous963, Thank you! Exactly what I needed. Who is right doesn't matter. What is right is all that matters.