I am just checking a Code calculation for tubes in a Section I boiler. The S values from 500 F to 800 F would be useful; I do have the 2010 Code values.

Many thanks in advance...

Who is right doesn't matter. What is right is all that matters.
 
Here you go:
[ul]
[li]Ambient to 650F: 15 ksi [/li]
[li]700: 14.4 ksi [/li]
[li]750: 13 ksi [/li]
[li]800F: 10.8 ksi [/li]
[/ul]
 
pdiculous963,

Thank you! Exactly what I needed.




Who is right doesn't matter. What is right is all that matters.
 