Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Looking for ASME II Part D 1995 S values SA106-B 1

Status
Not open for further replies.

SNORGY

Mechanical
Sep 14, 2005
2,510
I am just checking a Code calculation for tubes in a Section I boiler. The S values from 500 F to 800 F would be useful; I do have the 2010 Code values.

Many thanks in advance...

Who is right doesn't matter. What is right is all that matters.
 
Replies continue below

Recommended for you

Here you go:
[ul]
[li]Ambient to 650F: 15 ksi [/li]
[li]700: 14.4 ksi [/li]
[li]750: 13 ksi [/li]
[li]800F: 10.8 ksi [/li]
[/ul]
 
pdiculous963,

Thank you! Exactly what I needed.