I have been looking for a BAC qualified supplier for AMS4640 Al NI BR. Can anyone help?
 
Replies continue below

Recommended for you

Thanks, I sent them an RFQ so now we wait and see. I guess they have their own internal specs. I was unable to find any reference to AMS 4640
 
On the left - look at ALLOYS - AMPCO ALUMINIUM BRONZE - AMPCO 45
Ampco 45 meets the AMS 4640 spec.
 
Thanks, I'm waiting for a response to my RFQ. If they can certify to the AMS spec we are off and running.
 
Thanks again, got the quote and placed the order. This place rocks...
 