I am looking for a way to quickly estimate the force required to press a dowel into a hole so I can select a properly sized press. I have the pin size and material of both pin and housing. I am an applications engineer preparing quotes for assembly equipment and the data I have to work with is often minimal or not exact yet I want to avoid oversizing and overpricing.
 
Replies continue below

Recommended for you

What size dowel, how tight, how long,
what material, how deep must it
penetrate?
 
diamondjim
This particular application it's a 10mm hardened steel dowel in a aluminum housing, 10H7 hole (+.015/-0). I have to assume a standard metric pin which I know is slightly oversized, +.012. Length of engagement is 12mm. I have to assume max. inteference of .012mm to size my press.
 