Hi

I'm looking for 316H bar 6in dia for a project I have. It needs to have a min carbon content of .39%

Does anybody know of any sources?

I appreciate any help anybody can give me.
 
Replies continue below

Recommended for you

316H grade has typically carbon content of 0.04-0.10%. Perhaps you have made a typo error in requesting for minimum 0.39% carbon.
 