I will be conducting (2) PQR tests soon. 1" thick coupons, A656-80 to A514, and 1" thick A514-A514.
I will be using Figure 4.10 from D1.1, using B-U2a-GF from Figure 3.4, 1/4" root.
Does anybody have experience with these materials, in this thickness? Were you able to make transverse bends work, or did you have to go to the much larger longitudinal specimen?
Thanks in advance
I will be using Figure 4.10 from D1.1, using B-U2a-GF from Figure 3.4, 1/4" root.
Does anybody have experience with these materials, in this thickness? Were you able to make transverse bends work, or did you have to go to the much larger longitudinal specimen?
Thanks in advance