Does anyone know of any published studies for long term deflection recordings of concrete slabs. The only study i know of is this one by Ian Gilbert & Co?
R407: An experimental study of reinforced concrete flat slabs under sustained service loads
Arguing with an engineer is like wrestling with a pig in mud. After a while you realize that they like it
R407: An experimental study of reinforced concrete flat slabs under sustained service loads
Arguing with an engineer is like wrestling with a pig in mud. After a while you realize that they like it