etsen
Mechanical
- Sep 11, 2006
- 67
For a local metal loss assessment, the remaining life of piping elbows can be computed by using the method based upon computation of a minimum required thickness for the intended service conditions? For example, r=(t1-t2)/(2c)
where r=remaining life,years
t1 = the minimum remaining wall thickness determined at the time of inspection,mm
t2 = minimum required thickness required by code,mm
c=anticipated corrosion rate,mm/year.To be conservative,the anticipated corrosion rate is multiplied by 2.
where r=remaining life,years
t1 = the minimum remaining wall thickness determined at the time of inspection,mm
t2 = minimum required thickness required by code,mm
c=anticipated corrosion rate,mm/year.To be conservative,the anticipated corrosion rate is multiplied by 2.