A pressure vessel(Vertical Column/Tower) was designed and fabricated at shop and Hydro tested at shop. Subsequently due to transportation constraints, the job was split up (that is one category B joint was cut) and the job/Joint was subsequently welded at site with the same configurations, 100% RT, DPT in root pass and final pass, 100% UT with angle beam technique and maintaining dimensions etc within tolerance.
Instead of performing Hydro test of the full tower, is it permissible to perform Hydro test/Pneumatic test of only the Joint in Question by providing temporary cover and then subsequently remove the support and perform DPT at the support location.
Will this be acceptable to AI.
Instead of performing Hydro test of the full tower, is it permissible to perform Hydro test/Pneumatic test of only the Joint in Question by providing temporary cover and then subsequently remove the support and perform DPT at the support location.