Load ring - for welding for low temperatures

Status
Not open for further replies.

Paolo.I

Petroleum
Apr 9, 2019
7
A well-known supplier of welded load ring, claims to supply an S355J2+N with impact test at -45. shouldn't he call it S355J4 / J5?
Can S355 reach these temperatures?

Thanks in advance for your answers
 
Replies continue below

Recommended for you

Reaching those temperatures (-45°C ?) isn't a problem. Achieving the impact values is or can be.
What are the impact values? What does he supply? Big difference between 27J and 100+ J.
 


Eng. Paolo.I (Petroleum),

I think the thickness of the welded load ring should be in the range of 10-15 mm.. The following table is useful to see the allowable thk. vs steel grades..
MAX_permissible_steel_thk_g1t8pm.jpg
 