I'm an OEM who's shipping a heavy piece of equipment to China for installation in a warehouse. The original spec that my company provided (before I joined) called for floor loading of 9800 kg/m^2. Now, at the 11th hour, they're saying that the maximum floor loading is only 500 kg/m^2.
I just don't see how that could be accurate for it's such a small number. They're preparing to rework the floors at substantial expense but I don't think it's necessary. However, I don't have the expertise to determine it. I'm trying to rapidly find a CE that I can hire to advise me but until then I'm wondering if somebody can give me some guidance as to how to come up with an approximate loading (assuming good concrete, etc).
I'm told the floor is about 7" thick concrete over sand and stone. I do not know about rebar.
This is a large warehouse at a huge manufacturing facility whose other buildings have large equipment. This building has a 5-ton gantry crane in it so they obviously intended to move heavy things around.
My gut tells me the equipment is fine but I'd like to be able to calculate it within some safety factor.
--------------------
Bring back the HP-15
--------------------
I just don't see how that could be accurate for it's such a small number. They're preparing to rework the floors at substantial expense but I don't think it's necessary. However, I don't have the expertise to determine it. I'm trying to rapidly find a CE that I can hire to advise me but until then I'm wondering if somebody can give me some guidance as to how to come up with an approximate loading (assuming good concrete, etc).
I'm told the floor is about 7" thick concrete over sand and stone. I do not know about rebar.
This is a large warehouse at a huge manufacturing facility whose other buildings have large equipment. This building has a 5-ton gantry crane in it so they obviously intended to move heavy things around.
My gut tells me the equipment is fine but I'd like to be able to calculate it within some safety factor.
--------------------
Bring back the HP-15
--------------------