Regular type of vault (no gold bars etc), for typical safe deposit box use. Seems like heavy storage 250 psf should be adequate but if anyone has experience with specifying a load for this condition, I would love to hear it.
A project I am familiar with is using 8" thick, #6 @ 12" ea way, for a slab on grade. I believe this is a banking industry requirement to make it difficult to tunnel into it. The rest of the bank building floor slab (SOG) is 4" thick with WWR
I'm actually a little surprised. Banks tend to be big companies with lots of branches. Unless it's a little credit union, or something, I'd have expected them to have a design standard.
some one mentioned that ASTM F1090 & F1247 discuss vault design. I looked at both specs but they don't mention live load but they do discuss thie multiple layers of reinforcement.