Mar 22, 2011 #1 karlb New member Joined Nov 29, 2001 Messages 14 Location CA WOULD ANYONE HAVE INFORMATION ABOUT WHAT METALS AND/OR COATINGS THAT CAN BE USED WITH LiH WITHOUT SIGNIFICANT REACTION/CORROSION, ESPECIALLY AT TEMPERATURE. OR IF THERE IS LiH COMPATIBILITY TABLE AVAILABLE SOMEWHERE? THANKS
WOULD ANYONE HAVE INFORMATION ABOUT WHAT METALS AND/OR COATINGS THAT CAN BE USED WITH LiH WITHOUT SIGNIFICANT REACTION/CORROSION, ESPECIALLY AT TEMPERATURE. OR IF THERE IS LiH COMPATIBILITY TABLE AVAILABLE SOMEWHERE? THANKS
Mar 23, 2011 #2 micalbrch Mechanical Joined Jan 9, 2010 Messages 955 Location DE No idea about metals but PTFE is the only plastic I know which is resistant up to 100 °C at least. Upvote 0 Downvote
Mar 24, 2011 #3 dogtop Chemical Joined Jan 18, 2005 Messages 164 Location US What about Nickel (and ALL the alloys of Nickel)? HTH Upvote 0 Downvote