Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Lithium bromide chillers

Status
Not open for further replies.

zarnihein86

Chemical
May 17, 2019
1
Three lithium bromide chillers are used in my factory.Now,we are running one chiller and then we occur cooling water and chilled water temperatures are high about 104F.How can i solve this.
 
Replies continue below

Recommended for you

These are absorption units and you are going to hire a mechanic familiar with them to diagnose and repair them.

Tell your boss that anything you are going to do will only make more problems.
 
First off you’ll need to get clearer on what your specific issue is. Is it the cooling water temp, the heating water temp, or something you are certain is specific to a lithium bromide chiller
 
Check with a specialist to do a proper water analysis to identify what is going on your absorption chillers.

it worth to check the vacuum pump if it working properly or not...

All the best
AB
 